Physical Properties Metric English Comments
Density 3.679 g/cc
0.1329 lb/in³
Laminate Density
Hardwire 3S-23-12 High Density Composite
The 3S Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3S cord is used where balanced compressive and tensile strengths are required and re..