Polymer Property : Density = 4.43 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 4.43 g/cc
0.160 lb/in³
Kobe Steel KS6-4 Alpha-Beta Titanium Alloy, ASTM Gr. 5, Annealed
Nominal Composition: Ti-6 Al-4 V Applications: Aircraft parts, connecting rods, valve spring retainers, structural parts, golf club heads.Features:High strength, excellent balance between strength ..
Density 4.43 g/cc
0.160 lb/in³
Schott N-LAF36 Glass
Information Provided by SCHOTT North America, Inc.
Density 4.43 g/cc
0.160 lb/in³
Schott N-LASF40 Glass
Information Provided by SCHOTT North America, Inc.
Density 4.43 g/cc
0.160 lb/in³
Typical
TIMET TIMETAL® 5111 Titanium Alloy (Ti-5Al-1Sn-1Zr-1V-0.8Mo; ASTM Grade 32)
High Toughness, Heavy Section Weldable AlloyFeatures: A near alpha alloy with excellent weldability, seawater stress corrosion cracking resistance and high dynamic toughness. It is ideally suited f..
Density 4.43 g/cc
0.160 lb/in³
ATI Allegheny Ludlum Grade 23 (6-4 ELI) Titanium (UNS R56401)
The ELI grade has lower impurity limits than standard titanium 6-4.Uses: applications requiring excellent fracture toughness and fatigue strength, aircraft, structural components, biomedical.Mechani..
Density 4.43 g/cc
0.160 lb/in³
ATI Allegheny Ludlum Grade 5 Titanium 6Al-4V (UNS R56400)
Uses: blades, discs, rings, airframe, fasteners, components, vessels, cases, hubs, forgings.Mechanical property data below is typical of annealed samples at room temperature.Information provided by ..
Density 4.43 g/cc
0.160 lb/in³
ATI Allvac® 6-4 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Data provided by Allvac.Applications: Blades, discs, rings, airframe, fasteners, components. Vessels, cases, hubs, forgings. Standard, rotor/premium grades.
Density 4.43 g/cc
0.160 lb/in³
ATI Allvac® 6-4ELI Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal
Data provided by Allvac.Applications: Applications requiring excellent fracture toughness and fatigue strength; aircraft, structural components, biomedical.