Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.90 g/cc | 0.249 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP SH0700B PA12 LNP* Thermocomp* SH0700B is a compound based on Nylon 12 containing proprietary fillers. Added feature: High Specific Gravity |
|||
Density | 6.90 g/cc | 0.249 lb/in³ | |
American Elements Tin Oxide Nanopowder General DescriptionTin Oxide ( SnO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide Parti.. |
|||
Density | 6.90 - 7.30 g/cc | 0.249 - 0.264 lb/in³ | |
Alliance A-5S Alnico Magnetic Material |
|||
Density | 6.90 - 7.30 g/cc | 0.249 - 0.264 lb/in³ | |
Alliance A-8S Alnico Magnetic Material |
|||
Density | 6.90 - 7.30 g/cc | 0.249 - 0.264 lb/in³ | |
Alliance A-6S Alnico Magnetic Material |
|||
Density | 6.90 - 7.30 g/cc | 0.249 - 0.264 lb/in³ | |
Alliance A-2S Alnico Magnetic Material |