Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 7.11 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 7.11 g/cc
0.257 lb/in³
California Fine Wire Stablohm 825 Nickel Chromium Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Density 7.11 g/cc
0.257 lb/in³
California Fine Wire Stablohm 875 Chromium, Aluminum, and Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.