Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.10 - 7.30 g/cc | 0.257 - 0.264 lb/in³ | |
Pacific Sintered Materials FS-1601 Silicon Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC uses.All information provided by Pacific Sintered Metals. |
|||
Density | 7.10 - 7.30 g/cc | 0.257 - 0.264 lb/in³ | |
Pacific Sintered Materials FS-1602 Silicon Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC uses.All information provided by Pacific Sintered Metals. |
|||
Density | 7.10 - 7.30 g/cc | 0.257 - 0.264 lb/in³ | |
PSM Industries Pacific Sintered Metals Silicon Iron FS-1601 Powdered Metal DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC usesInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 7.10 - 7.30 g/cc | 0.257 - 0.264 lb/in³ | |
PSM Industries Pacific Sintered Metals Silicon Iron FS-1602 Powdered Metal DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC usesInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Density | 7.10 g/cc | 0.257 lb/in³ | |
Resistalloy International Fecralloy™ 145 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kiln.. |
|||
Density | 7.10 g/cc | 0.257 lb/in³ | |
Goodfellow Chromaloy O® Resistance Alloy Resistance heating alloy with excellent resistance to oxidation at elevated temperatures. Used in many varied applications - from small household appliances to large industrial furnaces.Information .. |
|||
Density | 7.10 g/cc | 0.257 lb/in³ | |
American Elements Gadolinium Oxide Nanopowder General DescriptionGD-MITE powders and dispersions are inorganic gadolinium-oxide nanoparticles. GD-MITE-A products are uncoated and hydrophilic. GD-MITE-O products are coated with an organic silane.. |
|||
Density | 7.10 g/cc | 0.257 lb/in³ | |
Goodfellow Aluchrom O® Resistance Alloy Resistance heating alloy with excellent resistance to oxidation at elevated temperatures. Used in many varied applications - from small household appliances to large industrial furnaces.Information .. |
|||
Density | 7.11 g/cc | 0.257 lb/in³ | |
California Fine Wire Stablohm 825 Nickel Chromium Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 7.11 g/cc | 0.257 lb/in³ | |
California Fine Wire Stablohm 875 Chromium, Aluminum, and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |