Physical Properties Metric English Comments
Density 7.31 g/cc
0.264 lb/in³
Indium Corp. Indalloy 88 Indium Solder Alloy
Information Provided by Indium Corporation
Density 7.31 g/cc
0.264 lb/in³
Indium Corp. Indalloy 90 Indium Solder Alloy
Information Provided by Indium Corporation
Density 7.31 g/cc
0.264 lb/in³
Indium Corp. Indalloy 91 Indium Solder Alloy
Information Provided by Indium Corporation
Density 7.31 g/cc
0.264 lb/in³
Indium Corp. Indalloy 92 Indium Solder Alloy
Information Provided by Indium Corporation
Density 7.31 g/cc
0.264 lb/in³
Indium Corp. Indalloy® 244 99.3Sn/0.7Cu Lead-Free Solder Alloy
Inexpensive. Alloy of choice for general wave solder assembly.Information provided by the manufacturer, Indium Corporation.
Density 7.31 g/cc
0.264 lb/in³
Indium Corp. Indalloy® 4 Pure Indium Solder
Soft, ductile metal has good wettability on many surfaces including ceramics, glass and quartz. Deforms indefinitely under load and has no tendency to become brittle, making it valuable for cryogeni..
Density 7.31 g/cc
0.264 lb/in³
Indium Corp. Indalloy 243 Tin Solder Alloy
Lead-free alloy, no PatentInformation Provided by Indium Corporation
Density 7.31 g/cc
0.264 lb/in³
Indium Corp. Indalloy® 263 Tin-Silver-Copper Solder Alloy
Information provided by the manufacturer, Indium Corporation of America.
Density 7.31 g/cc
0.264 lb/in³
Williams Advanced Alloys WS157 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Density 7.31 g/cc
0.264 lb/in³
American Elements Indium Nanoparticles
General DescriptionIndium (In) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Indium Particles are typically 20-40 nanomete..
Density 7.31 g/cc
0.264 lb/in³
American Elements Tin Nanoparticles
General DescriptionTin (Sn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Tin Particles are typically 10-20 nanometers (nm) with specifi..
Density 7.31 g/cc
0.264 lb/in³
California Fine Wire Stablohm 750 Chromium, Aluminum, and Iron Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Density 7.31 g/cc
0.264 lb/in³
AIM 100In Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Density 7.31 g/cc
0.264 lb/in³
Indium Corp. Indalloy 225 Indium Solder Alloy
Information Provided by Indium Corporation