Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.78 g/cc | 0.281 lb/in³ | |
Misumi G-STAR Martensite Free-cutting Stainless Steel Corrosion resistant; excellent machinability. Comparable in material properties and chemical make up to STAVAX mold steel.Information provided by MISUMI Corporation. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Latrobe Lescowearâ„¢ Cold Work Tool Steel Lescowear cold work tool steel is a versatile medium-chromium, air-hardening tool steel that is characterized by a very good combination of toughness and wear resistance. It is available primarily i.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Latrobe LSSâ„¢ A9 Tool Steel (ASTM A9) TLS A9 tool steel is a 5% chromium tool steel with a unique combination of properties which make it suitable for both cold work and hot work tooling applications. The combination of nickel, vanadium.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Latrobe LSSâ„¢ H10A Modified TLS H10 Mod. hot work tool steel is a chromium-molybdenum H10-type hot work steel which contains cobalt for increased strength and resistance to softening at elevated temperature. This grade is also.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Indium Corp. Indalloy® 238 Sn-Au Solder Alloy Lower temp eutectic, in the Au Sn system.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Latrobe 14-4CrMo Stainless Tool Steel 14-4CrMo is a wear resistant, martensitic stainless tool steel that exhibits better corrosion resistance than Type 440C stainless steel. The molybdenum in the steel provides superior corrosion resis.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel Description: Thermodur® 2367 Superclean is an electro slag remelted (ESR) hot work die steel developed for applications where high temperature properties (tensile strength & thermal conductivity).. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Crucible Steel 161 Tool Steel, High Carbon H13 Crucible 161 is a high carbon modification of H13, intended for applications requiring higher hardness, compressive strength, wear resistance, or tempering resistance (hot hardness), at slightly low.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Crucible Steel CHRO-MOW® Tool Steel, AISI H12 Chro-Mow is a general purpose hot work tool steel, combining good high-temperature strength with moderate toughness and heat check resistance. It is suited for applications where drastic coolants ar.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Crucible Steel CPM® 154 Tool Steel CPM 154 is CPM-manufactured version of Crucible’s standard 154 CM. The CPM manufacturing process produces a uniform distribution of the carbides in this grade, giving this CPM 154 easier grinding a.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM DIEVAR® Hot Work Tool Steel Description: Uddeholm Dievar is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross cracking, hot wear and plastic.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM QRO® 90 SUPREME Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelQRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum.. |
|||
Density | 7.78 g/cc @Temperature 599 °C |
0.281 lb/in³ @Temperature 1110 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 23 (AISI M3:2) Hot Work Tool Steel Chromium-molybdenum-tungsten-vanadium alloyed PM steelVanadis 23 is a high speed powder metallurgical steel, recommended for low temperature die casting applications and warm forging applications wh.. |
|||
Density | 7.78 g/cc @Temperature 600.0 °C |
0.281 lb/in³ @Temperature 1112 °F |
soft annealed |
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W .. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition A AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
Density | 7.78 g/cc @Temperature 600 °C |
0.281 lb/in³ @Temperature 1110 °F |
soft annealed condition |
Assab Steels ASP 60 Cold Work Steel ASP 60 is a W-Mo-V-Co alloyed PM high speed steel characterized by:Highest wear resistanceMaximum compressive strengthGood through hardening propertiesGood toughnessGood dimensional stability on hea.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Assab Steels CALMAX Plastic Mold Material CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Assab Steels 8407 2M Hot Work Steel ASSAB 8407 is a chromium-molybdenum-vanadium-alloyed steel which is characterized by: Good resistance to abrasion at both low and high temperatures. High level of toughness and ductility Uniform .. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Assab Steels HOTVAR Hot Work Steel HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
ATI Allvac® M-50 Specialty Steel, Heat Treatment: 1107°C (2025°F) Q+T Data provided by Allvac.Applications: Bearing applications, including turbine engine main shaft bearings. Cutting tools. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
ATI Allvac® Nickelvac® D6AC UNS K24728 Specialty Steel Uses: High performance aircraft structural parts.Property values are for samples in the metallurgical condition: 1550°F Q + 1000°F T.Information provided by Allvac, An Allegheny Teledyne Company. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
ATI Allvac® Vasco® 17-4 Precipitation Hardening Steel, Heat Treatment: 1038°C (1900°F) + Age Data provided by Allvac.Applications: Aircraft and missile fittings, fasteners, gears. Turbine and pump blades, shafts. |
|||
Density | 7.78 g/cc @Temperature 600 °C |
0.281 lb/in³ @Temperature 1110 °F |
|
Assab Steels ASP 23 Cold Work Steel ASP 23 is a chromium-molybdenum-tungsten-vanadium alloyed high speed steel which is characterized by:High wear resistance (abrasive profile)High compressive strengthVery good through-hardening prope.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
ATI Allegheny Ludlum AL 15-5 High Strength Stainless Steel, UNS S15500 Property data below is typical of annealed samples. Available in plate. For use in fasteners, military equipment and air frame parts.Information provided by Allegheny Ludlum |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Latrobe Lescalloy® HY-TUF VAC-ARC High Strength Alloy Steel LESCALLOY HY-TUF VAC-ARC steel is a high strength low alloy steel. It is typically used in the 220/240 ksi (1517/1655 MPa) tensile strength range. At this strength level, the alloy has good ductilit.. |
|||
Density | 7.78 g/cc | 0.281 lb/in³ | |
Schmolz + Bickenbach Thermodur® 2344 EFS Extra Fine Structure - Hot Work Die Steel Description: THERMODUR 2344 is a single melt Extra Fine Structure (EFS) hot work die steel; and Supplied in the annealed conditionCharacteristics: Good toughness; Good resistance to thermal shock a.. |