Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.90 g/cc | 0.285 lb/in³ | RT |
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and ro.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | RT |
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | RT |
Outokumpu 4541 Cr-Ni Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto), hot rolled strip/sheet (C.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | RT |
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
Industeel CLC 18.10 L General Purpose 18Cr-10Ni Austenitic Stainless Steel Description: CLC 18-10L is a 18Cr-10Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenchi.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
Industeel SIRIUS S12 20% Cr - 1.8% Si Heat Resistant Steel Description: CLI SIRIUS S12 grade is an austenitic stainless steel containing 20% Cr, 1.8 % Si and 12% Ni. The low nickel content combined with high chromium and high silicon contents provide good r.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
Industeel URANUS® 65 310 L Modified Grade - Low C and Si for Nitric Acid Service Description: URANUS® 65 is a 25 Cr 20 Ni austenitic stainless steel with sharp control of the residual elements in order to provide high corrosion resistance properties in boiling 50-65% Nitric a.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 40% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 10% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 50% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 0% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 40% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, Annealed (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 50% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 60% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel AL 904L™ Alloy (UNS N08904) Allegheny Ludlum AL 904 L™ Alloy (UNS N08904) is an austenitic stainless steel alloy designed for a middles to high level of corrosion resistance. The alloy is produced to low carbon levels for us.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 0% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 60% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 30% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
Resistalloy International Resistalloy 3718 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |
|||
Density | 7.90 g/cc | 0.285 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 60% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |