Polymer Property : Density = 9.97 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 9.97 g/cc
0.360 lb/in³
Indium Corp. Indalloy 48 Bismuth Solder Alloy
Information Provided by Indium Corporation
Density 9.97 g/cc
0.360 lb/in³
Indium Corp. Indalloy® 10 Pb-In Solder Alloy
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics..
Density 9.97 g/cc
0.360 lb/in³
Williams Advanced Alloys WS264 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys