Material Notes:
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics of lead-indium as well as good thermal fatigue properties.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 9.97 g/cc
0.360 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 10.2

@Load 100 kg,
Time 30.0 sec
10.2

@Load 220 lb,
Time 0.00833 hour
Tensile Strength, Ultimate 37.6 MPa
5450 psi
Elongation at Break 47.5 %
47.5 %
Shear Strength 24.3 MPa
3520 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 26.0 µm/m-°C

@Temperature 20.0 °C
14.4 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 18.0 W/m-K

@Temperature 85.0 °C
125 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 240 - 260 °C
464 - 500 °F
Solidus 240 °C
464 °F
Liquidus 260 °C
500 °F
Component Elements Properties Metric English Comments
Indium, In 25 %
25 %
Lead, Pb 75 %
75 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000370 ohm-cm
0.0000370 ohm-cm