Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 1.3 cSt | 1.3 cSt | ASTM D445 |
ExxonMobil Varsolâ„¢ 18 Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: North America and South AmericaInformation provided by ExxonMobil |