Polymer Property : Kinematic Viscosity = 1.3 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity 1.3 cSt
1.3 cSt
ASTM D445
ExxonMobil Varsolâ„¢ 18 Non-dearomatized Fluid
Appearance: Clear/Transparent LiquidAvailability: North America and South AmericaInformation provided by ExxonMobil