Polymer Property : Neck In = 13.5 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Neck In 13.5 cm
5.31 in
610°F and 1.0 mil; Extrusion Coating Processability; Dow Method
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin
AFFINITY™ PT 1450G1 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. The resin is for monolayer and co-extrusion coating that offers excellent low temperature seal initiation, ult..