Physical Properties Metric English Comments
Drawdown 9.00 m/s

@Temperature 230 °C
1770 ft/min

@Temperature 446 °F
Constant output at 35 rpm; ExxonMobil Method
ExxonMobil Escorene™ LD 726.07 Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 726.07 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. LD 716.07 is an excelle..