Polymer Property : Drawdown = 4.00 m/s Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Drawdown 4.00 m/s

@Temperature 280 °C
787 ft/min

@Temperature 536 °F
Constant output at 35 rpm; ExxonMobil Method
ExxonMobil Escor™ 5100 ExCo Ethylene Acrylic Acid Copolymer Resin
Product Description: Escor 5100 is primarily intended for extrusion coating, coextrusion coating and extrusion lamination. Excellent adhesion to polar substrates, aluminum foil, metalized films, pap..
Drawdown 4.00 m/s
787 ft/min
ExxonMobil Method
ExxonMobil LD 202.48 Extrusion Coating Resin
Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro..
Drawdown 4.00 m/s
787 ft/min
Constant output at 35 rpm; ExxonMobil Method
ExxonMobil LDPE LD 202.48 Low Density Polyethylene Resin
Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro..
Drawdown 4.00 m/s

@Temperature 315 °C
787 ft/min

@Temperature 599 °F
Constant output at 35 rpm; ExxonMobil Method
ExxonMobil LDPE LD 251 Low Density Polyethylene Resin (European Grade)
Product Description: LD 251 is an LDPE extrusion coating grade, offering:low neck-in excellent heat sealablity (ie high seal speeds and/or seal temperatures mostly required in high speed form-fill a..