Physical Properties | Metric | English | Comments |
---|---|---|---|
Drawdown | 4.00 m/s @Temperature 280 °C |
787 ft/min @Temperature 536 °F |
Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil Escor™ 5100 ExCo Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5100 is primarily intended for extrusion coating, coextrusion coating and extrusion lamination. Excellent adhesion to polar substrates, aluminum foil, metalized films, pap.. |
|||
Drawdown | 4.00 m/s | 787 ft/min | ExxonMobil Method |
ExxonMobil LD 202.48 Extrusion Coating Resin Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro.. |
|||
Drawdown | 4.00 m/s | 787 ft/min | Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil LDPE LD 202.48 Low Density Polyethylene Resin Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro.. |
|||
Drawdown | 4.00 m/s @Temperature 315 °C |
787 ft/min @Temperature 599 °F |
Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil LDPE LD 251 Low Density Polyethylene Resin (European Grade) Product Description: LD 251 is an LDPE extrusion coating grade, offering:low neck-in excellent heat sealablity (ie high seal speeds and/or seal temperatures mostly required in high speed form-fill a.. |