Polymer Property : Drawdown = 689 ft/min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Drawdown 3.50 m/s
689 ft/min
Constant output at 35 rpm; ExxonMobil Method
ExxonMobil Escor™ 6000 ExCo Ethylene Acrylic Acid Copolymer Resin
Product Description: Escor 6000 is primarily intended for extrusion coating and coextrusion coating. Escor 6000 is the high draw down version of Escor 5000. Very low coating weight achievable at hig..