Physical Properties | Metric | English | Comments |
---|---|---|---|
Drawdown | 8.17 m/s @Temperature 230 °C |
1610 ft/min @Temperature 446 °F |
Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil Escorene™ FL 01418 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 01418 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. FL 01418 is an excellent sealing materi.. |