Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 11.4 g/m² | 7.10 lb/ream | ExxonMobil Method |
ExxonMobil Bicor® 50 LBW OPP Film Product Description: Bicor LBW is a two-sided treated, slip modified, non-heat sealable OPP film designed for use as the outside web of a lamination. The print surface is treated and can be printed .. |
|||
Coating Weight | >= 11.4 g/m² | >= 7.10 lb/ream | 520 |
ExxonMobil Label-Lyte® 612 LLG-102 Clear OPP Film Clear, polypropylene films designed for use in roll-fed labeling applications. This film can be laminated to itself or applied as an outer web to other films. The print surface is a treated high ene.. |
|||
Coating Weight | 11.4 g/m² | 7.10 lb/ream | ExxonMobil Method |
ExxonMobil Label-Lyte™ 612LLG102 OPP Film Product Description: A clear, two-side treated, polypropylene film that is used in roll-fed labeling applications. This film can be laminated to itself or applied as an outer web to other films. 612.. |
|||
Coating Weight | 11.4 g/m² | 7.10 lb/ream | ExxonMobil Method |
ExxonMobil Metallyte® 50 TSPM OPP Film Product Description: A high barrier, non-sealable OPP film with one-side metalized a one-side treated. TSP< is designed for use as the inner web of a cold seal lamination or as the center web of a t.. |
|||
Coating Weight | 11.4 g/m² | 7.10 lb/ream | ExxonMobil Method |
ExxonMobil Metallyte™ 12MM281 OPP Film Product Description: A high barrier, non-sealable OPP film with one-side metalized and one-side treated. 12MM281 is designed for use as the center web of a triplex adhesive lamination. The treated s.. |
|||
Coating Weight | >= 11.4 g/m² | >= 7.10 lb/ream | 520 |
ExxonMobil Label-Lyte® 612 LL-112 Clear OPP Overlaminate Clear, polypropylene film designed to provide exceptional clarity and print protection when used as an overlaminate in pressure-sensitive labeling applications. The treated high energy layer provide.. |