Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | >= 6.40 g/m² | >= 4.00 lb/ream | TAPPI test method; ASTM D539 |
NOVA Chemicals Novapol® LC-0717-A LDPE Extrusion Resin High speeds, Low coating weights, Excellent adhesion, Excellent drawdown, Excellent sealabilityApplications: Sugar pouch stock; Popsicle wrap, Multi-wall bags, High speed/low coating weight paper co.. |
|||
Coating Weight | >= 6.40 g/m² | >= 4.00 lb/ream | Extrusion Coating Processability; Dow Method |
Dow 4012 Low Density Polyethylene (LDPE) Polyethylene 4012 is used for a variety of applications such as condiment packaging, dry and moist foods packaging, sugar pouches, lidding stock and medical packaging.Information provided by Dow |