Polymer Property : Coating Weight = 6.40 g/m² Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight >= 6.40 g/m²
>= 4.00 lb/ream
TAPPI test method; ASTM D539
NOVA Chemicals Novapol® LC-0717-A LDPE Extrusion Resin
High speeds, Low coating weights, Excellent adhesion, Excellent drawdown, Excellent sealabilityApplications: Sugar pouch stock; Popsicle wrap, Multi-wall bags, High speed/low coating weight paper co..
Coating Weight >= 6.40 g/m²
>= 4.00 lb/ream
Extrusion Coating Processability; Dow Method
Dow 4012 Low Density Polyethylene (LDPE)
Polyethylene 4012 is used for a variety of applications such as condiment packaging, dry and moist foods packaging, sugar pouches, lidding stock and medical packaging.Information provided by Dow