Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | >= 7.20 g/m² | >= 4.50 lb/ream | Extrusion Coating Processability; Dow Method |
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin AFFINITY™ PT 1450G1 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. The resin is for monolayer and co-extrusion coating that offers excellent low temperature seal initiation, ult.. |