Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0032 - 0.0041 cm/cm

@Time 86400 sec
0.0032 - 0.0041 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE003 PC (Asia Pacific)
LNP STAT-KON* DE003 is a compound based on Polycarbonate resin containing Carbon Fiber.
Linear Mold Shrinkage, Transverse 0.0032 - 0.0041 cm/cm

@Time 86400 sec
0.0032 - 0.0041 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE003ER PC
LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive.
Linear Mold Shrinkage, Transverse 0.0032 - 0.0041 cm/cm

@Time 86400 sec
0.0032 - 0.0041 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE003P PC (Asia Pacific)
LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0032 - 0.0041 cm/cm

@Time 86400 sec
0.0032 - 0.0041 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE003ER PC (Asia Pacific)
LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0032 - 0.0041 cm/cm

@Time 86400 sec
0.0032 - 0.0041 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DE003P PC