Polymer Property : Linear Mold Shrinkage, Transverse = 0.0052 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0052 cm/cm

@Time 86400 sec
0.0052 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI
LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Linear Mold Shrinkage, Transverse 0.0052 cm/cm

@Time 86400 sec
0.0052 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific)
LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Linear Mold Shrinkage, Transverse 0.0052 cm/cm

@Time 86400 sec
0.0052 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Verton NV006E PC/ABS
LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas region..
Linear Mold Shrinkage, Transverse 0.0052 cm/cm

@Time 86400 sec
0.0052 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON NV006E PC/ABS (Asia Pacific)
LNP* Verton* NV006E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Transverse 0.0052 cm/cm

@Time 86400 sec
0.0052 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON NV006E PC+ABS
LNP* Verton* NV006E is a compound based on PC+ABS blend resin containing 30% Long Glass Fiber. Added features of this material include: Easy Molding, Structural.