Polymer Property : Linear Mold Shrinkage, Transverse = 0.0081 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0081 cm/cm

@Time 86400 sec
0.0081 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRILOY D2000 PC
LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0081 cm/cm

@Time 86400 sec
0.0081 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRILOY D2000P PC
LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing, Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0081 cm/cm

@Time 86400 sec
0.0081 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRILOY D2000P PC (Asia Pacific)
LNP LUBRILOY* D2000P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Exceptional Processing.
Linear Mold Shrinkage, Transverse 0.0081 cm/cm

@Time 86400 sec
0.0081 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR
LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Linear Mold Shrinkage, Transverse 0.0081 cm/cm

@Time 86400 sec
0.0081 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR (Asia Pacific)
LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.