Linear Mold Shrinkage, Transverse 0.0115 cm/cm

@Time 86400 sec
0.0115 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXY PA 66
LNP* LUBRICOMP* RFL36XXY is a compound based on Nylon 66 containing 30% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0115 cm/cm

@Time 86400 sec
0.0115 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubriloy Z2000 PPE+PS
LNP* Lubriloy* Z2000 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP fo..
Linear Mold Shrinkage, Transverse 0.0115 cm/cm

@Time 86400 sec
0.0115 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubriloy Z2000 PPE+PS
LNP* Lubriloy* Z2000 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP fo..
Linear Mold Shrinkage, Transverse 0.0115 cm/cm

@Time 86400 sec
0.0115 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY Z2000 PPE+PS (Asia Pacific)
LNP* Lubriloy* Z2000 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0115 cm/cm

@Time 86400 sec
0.0115 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRILOY Z2000 PPE+PS (Asia Pacific)
LNP* Lubriloy* Z2000 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.0115 cm/cm

@Time 86400 sec
0.0115 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY Z2000 PPO
LNP* LUBRILOY* Z2000 is a compound based on PPO resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0115 cm/cm

@Time 86400 sec
0.0115 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRILOY Z2000 PPO
LNP* LUBRILOY* Z2000 is a compound based on PPO resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.0115 cm/cm

@Time 86400 sec
0.0115 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON PFD06 PA 6
LNP* STAT-KON* PFD06 is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0115 cm/cm

@Time 86400 sec
0.0115 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON PFD06 PA 6 (Asia Pacific)
LNP* Stat-kon* PFD06 is a compound based on Nylon 6 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0115 cm/cm

@Time 86400 sec
0.0115 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP
LNP THERMOCOMP* MB006S is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized.