Material Notes:
LNP* Stat-kon* PFD06 is a compound based on Nylon 6 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Moisture Absorption 0.500 %
0.500 %
50% RH, 24 hrs; ASTM D570
0.910 %
0.910 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0038 cm/cm

@Time 86400 sec
0.0038 in/in

@Time 24.0 hour
ISO 294
0.0040 cm/cm

@Time 86400 sec
0.0040 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0115 cm/cm

@Time 86400 sec
0.0115 in/in

@Time 24.0 hour
ISO 294
0.012 cm/cm

@Time 86400 sec
0.012 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 159 MPa
23100 psi
ASTM D638
Elongation at Break 2.3 %
2.3 %
ASTM D638
Tensile Modulus 11.72 GPa
1700 ksi
50 mm/min; ASTM D638
Flexural Strength 241 MPa
35000 psi
ASTM D790
Flexural Modulus 11.03 GPa
1600 ksi
ASTM D790
Izod Impact, Notched 1.06 J/cm
1.99 ft-lb/in
ASTM D256
Izod Impact, Unnotched 9.07 J/cm
17.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 206 °C

@Thickness 3.20 mm
403 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
ASTM D257
Surface Resistance 1.0 - 6.0 ohm
1.0 - 6.0 ohm
ASTM D257