Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer
LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer
LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly
LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly
LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10
LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am..
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As..
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp KB005 Acetal Copolymer
LNP THERMOCOMP* KB005 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp 2C004
LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup..
Linear Mold Shrinkage, Transverse 0.022 cm/cm

@Time 86400 sec
0.022 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE
LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.