Polymer Property : Linear Mold Shrinkage, Transverse = 0.023 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.023 cm/cm

@Time 86400 sec
0.023 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer
LNP* LUBRICOMP* KL001 is a compound based on Acetal Copolymer resin containing 5% PTFE. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.023 cm/cm

@Time 86400 sec
0.023 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer
LNP* LUBRICOMP* KL001 is a compound based on Acetal Copolymer resin containing 5% PTFE. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.023 cm/cm

@Time 86400 sec
0.023 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KL001 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.023 cm/cm

@Time 86400 sec
0.023 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP KL001 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KL001 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.023 - 0.025 cm/cm

@Time 86400 sec
0.023 - 0.025 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly
LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible.
Linear Mold Shrinkage, Transverse 0.023 - 0.025 cm/cm

@Time 86400 sec
0.023 - 0.025 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KP004L is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.
Linear Mold Shrinkage, Transverse 0.023 cm/cm

@Time 86400 sec
0.023 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal
LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.023 cm/cm

@Time 86400 sec
0.023 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal (Asia Pacific)
LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.023 cm/cm

@Time 86400 sec
0.023 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY K2000XXH Acetal
LNP LUBRILOY* K2000XXH is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material are: Wear Resistant, Healthcare.
Linear Mold Shrinkage, Transverse 0.023 - 0.025 cm/cm

@Time 86400 sec
0.023 - 0.025 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66
LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.023 - 0.025 cm/cm

@Time 86400 sec
0.023 - 0.025 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66 (Asia Pacific)
LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.