Polymer Property : Linear Mold Shrinkage, Transverse = 0.023 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.021 - 0.023 cm/cm

@Time 86400 sec
0.021 - 0.023 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10
LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am..
Linear Mold Shrinkage, Transverse 0.021 - 0.023 cm/cm

@Time 86400 sec
0.021 - 0.023 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As..
Linear Mold Shrinkage, Transverse 0.0214 - 0.023 cm/cm

@Time 86400 sec
0.0214 - 0.023 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT
LNP LUBRICOMP* WL004 is a compound based on PBT resin containing 20% PTFE. Added features of this material include: Wear Resistant.