Physical Properties Metric English Comments
Viscosity Measure 2.9 cSt
2.9 cSt
internal phase
Dow Corning FZ-3196 Caprylyl Methicone
Dow Corning® FZ-3196 is a unique solution for formulators of skin care, sun care, or color cosmetic products. Caprylyl Methicone combines a light, silky feel, excellent spreadability and moderate v..