Dow Corning FZ-3196 Caprylyl Methicone

Category Polymer , Thermoplastic , Siloxane
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning FZ-3196 Caprylyl Methicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning® FZ-3196 is a unique solution for formulators of skin care, sun care, or color cosmetic products. Caprylyl Methicone combines a light, silky feel, excellent spreadability and moderate volatility with excellent compatibility with a wide range of cosmetic ingredients (such as natural oils), of which it improves the overall sensory profile by reducing greasiness and tackiness. It is a caprylyl branched trisiloxane. The siloxane consists of three silicon atoms which is the shortest Dimethicone, and octyl group is attached on the middle silicon.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.840 g/cc

@Temperature 25.0 °C
0.840 g/cc

@Temperature 77.0 °F
Volatiles 100 %
100 %
Viscosity Measure 2.9 cSt
2.9 cSt
internal phase
Surface Tension 20.4 dynes/cm
20.4 dynes/cm
Thermal Properties Metric English Comments
Flash Point 110 °C
230 °F
closed cup
Optical Properties Metric English Comments
Refractive Index 1.413
1.413