Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 250000 - 580000 cSt | 250000 - 580000 cSt | Kinetic/Kinematic |
Dow Corning 9040 Silicone Elastomer Blend A mixture of high molecular weight silicone elastomers (dimethicone crosspolymer) in cyclopentasiloxane for use in skincare, haircare, color cosmetics, suncare, antiperspirants and deodorants, and w.. |