Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 7.50 cm @Thickness 1.00 mm |
2.95 in @Thickness 0.0394 in |
395°C nozzle, 200°C tool |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |