Polymer Property : Spiral Flow = 7.50 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 7.50 cm

@Thickness 1.00 mm
2.95 in

@Thickness 0.0394 in
395°C nozzle, 200°C tool
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.