Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 9.00 cm @Thickness 1.00 mm |
3.54 in @Thickness 0.0394 in |
415°C nozzle, 210°C tool |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |
|||
Spiral Flow | 9.00 cm @Thickness 1.00 mm |
3.54 in @Thickness 0.0394 in |
405°C nozzle, 190°C tool |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |