Polymer Property : Bulk Density = 0.000289 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.00800 - 0.300 g/cc
0.000289 - 0.0108 lb/in³
BASF Neopolen® P 92HD 105 Expanded Polypropylene (Europe)
Description: Neopolen® P 92HD 105 is expanded Polypropylene supplied in the form of beads. The cells are largely closedInformation provided by BASF