BASF Neopolen® P 92HD 105 Expanded Polypropylene (Europe)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Foamed
Manufacturer BASF
Trade Name Neopolen®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Neopolen® P 92HD 105 Expanded Polypropylene (Europe).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Neopolen® P 92HD 105 is expanded Polypropylene supplied in the form of beads. The cells are largely closedInformation provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.00800 - 0.300 g/cc
0.000289 - 0.0108 lb/in³
Density 0.0100 - 0.400 g/cc

@Pressure 0.101 MPa,
Temperature 20.0 °C
0.000361 - 0.0145 lb/in³

@Pressure 14.7 psi,
Temperature 68.0 °F
Thermal Properties Metric English Comments
Melting Point 120 - 180 °C
248 - 356 °F
Decomposition Temperature >= 180 °C
>= 356 °F
Flash Point >= 200 °C
>= 392 °F
ASTM D 1929
Descriptive Properties Value Comments
Commercial Status Europe
Ignition Temperature > 360 °C
ASTM D1929