Physical Properties Metric English Comments
Bulk Density 0.0230 g/cc
0.000831 lb/in³
Minimum
SYNTHOS Koplen® 1020 FR Expandable Polystyrene
Low Pentane Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into thick walled products and blocks. Lower density can be ach..
Bulk Density 0.0230 g/cc
0.000831 lb/in³
Minimum
SYNTHOS Koplen® 1640 FR Expandable Polystyrene
Low Pentane Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks. Lower density can be achieved after several prefor..