Physical Properties Metric English Comments
Bulk Density 0.192 - 0.256 g/cc
0.00694 - 0.00926 lb/in³
Loose
KaMin KaMin® 80 Kaolin Clay - Waterwashed
KaMin® 80 is an economical, general purpose water-washed kaolin, with intermediate brightness. It is suitable for use in water-borne, solvent-borne and solvent-free paint, ink, and adhesive appli..
Bulk Density 0.192 - 0.256 g/cc
0.00694 - 0.00926 lb/in³
Loose
KaMin Polyfil® X Kaolin Clay - Waterwashed
Cost effective, kaolin extender offering improved consistency vs air floated clays, pulverized powder form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, SMC/BMC, EPDM, Mold..