KaMin KaMin® 80 Kaolin Clay - Waterwashed

Category Ceramic , Clay , Kaolin Clay
Manufacturer KaMin LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KaMin KaMin® 80 Kaolin Clay - Waterwashed.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KaMin® 80 is an economical, general purpose water-washed kaolin, with intermediate brightness. It is suitable for use in water-borne, solvent-borne and solvent-free paint, ink, and adhesive applications. Industry: Paint & Coatings, Adhesives & SealantsUses: Architectural Coatings, Industrial Coatings, Flat/Matte, Satin, Tinting Paste, Water Based, Solvent Borne,Information provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.192 - 0.256 g/cc
0.00694 - 0.00926 lb/in³
Loose
Brightness 87 %
87 %
Reflectance (TAPPI)
Oil Absorption 42 %
42 %
Fineness >= 5
>= 5
Hegman Grind
Moisture Absorption at Equilibrium <= 1.5 %
<= 1.5 %
As Produced
Particle Size 0.500 µm
0.500 µm
Average Stokes Equivalent Diameter
2.50 µm
2.50 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 7
7
100 g/250 ml H2O Slurry
Specific Surface Area 16.0 m²/g
16.0 m²/g
BET
Descriptive Properties Value Comments
Bulking Value 21.7 lb.gal
CAS Number 1332-58-7
Crystalline Silica (quartz) <0.1%
Physical Form Dry
Shipping Point Macon, GA