Physical Properties Metric English Comments
Bulk Density 0.462 g/cc
0.0167 lb/in³
ISO 1183
SABIC Innovative Plastics PPO 630 PPO (Asia Pacific)
PPO* 630 resin is a medium molecular weight polymer based on Polyphenylene Ether (PPE). PPO* is intended for use as an additive or a building block in a variety of thermoplastics and thermoplastic e..
Bulk Density 0.462 g/cc
0.0167 lb/in³
ISO 1183
SABIC Innovative Plastics PPO 630 PPO
PPO* 630 resin is a medium molecular weight polymer based on Polyphenylene Ether (PPE). PPO* is intended for use as an additive or a building block in a variety of thermoplastics and thermoplastic e..
Bulk Density 0.462 g/cc
0.0167 lb/in³
ISO 1183
SABIC Innovative Plastics PPO 630 PPO (Europe-Africa-Middle East)
PPO* 630 resin is a medium molecular weight polymer based on Polyphenylene Ether (PPE). PPO* is intended for use as an additive or a building block in a variety of thermoplastics and thermoplastic e..