Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.462 g/cc | 0.0167 lb/in³ | ISO 1183 |
SABIC Innovative Plastics PPO 630 PPO (Asia Pacific) PPO* 630 resin is a medium molecular weight polymer based on Polyphenylene Ether (PPE). PPO* is intended for use as an additive or a building block in a variety of thermoplastics and thermoplastic e.. |
|||
Bulk Density | 0.462 g/cc | 0.0167 lb/in³ | ISO 1183 |
SABIC Innovative Plastics PPO 630 PPO PPO* 630 resin is a medium molecular weight polymer based on Polyphenylene Ether (PPE). PPO* is intended for use as an additive or a building block in a variety of thermoplastics and thermoplastic e.. |
|||
Bulk Density | 0.462 g/cc | 0.0167 lb/in³ | ISO 1183 |
SABIC Innovative Plastics PPO 630 PPO (Europe-Africa-Middle East) PPO* 630 resin is a medium molecular weight polymer based on Polyphenylene Ether (PPE). PPO* is intended for use as an additive or a building block in a variety of thermoplastics and thermoplastic e.. |