Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | Loose |
Nyco M15 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | Loose |
Nyco M3 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | Loose |
Nyco NYAD® 1250 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | Loose |
Nyco NYCOR® R Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | Tapped |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | Tapped |
Nyco RRIMGLOS® II Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Bulk Density | 0.480 - 0.540 g/cc | 0.0173 - 0.0195 lb/in³ | PVCH/QCD/3516 |
Reliance Industries 57-01 Polyvinyl Chloride Information provided by Reliance IndustriesApplications: Rigid injection. |
|||
Bulk Density | 0.480 - 0.540 g/cc | 0.0173 - 0.0195 lb/in³ | PVCH/QCD/3516 |
Reliance Industries 60-11 Polyvinyl Chloride Information provided by Reliance IndustriesApplications:Recommended:Rigid extrusionRigid injectionRigid calenderingCan be used:Blow molding |
|||
Bulk Density | 0.480 - 0.540 g/cc | 0.0173 - 0.0195 lb/in³ | PVCH/QCD/3516 |
Reliance Industries 67-11 Polyvinyl Chloride Information provided by Reliance IndustriesApplications: Recommended:Flexible extrusionFlexible injectionFlexible calenderingCan be used:Rigid injectionRigid extrusion |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | |
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | |
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Bulk Density | 0.480 - 0.540 g/cc | 0.0173 - 0.0195 lb/in³ | PVCH/QCD/3516 |
Reliance Industries 57-11 Polyvinyl Chloride Information provided by Reliance IndustriesApplications: Rigid injectionRigid extrusionRigid calenderingblow molding |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | ISO 12086 |
3M Dyneon™ TF 2029 PTFE
(discontinued **) Processable by standard paste extrusion methodsDesigned for low reduction ratiosCan be processed at a high stretch ratiosRecommended for apes requiring high mechanical strength, such as electrical t.. |
|||
Bulk Density | 0.480 - 0.560 g/cc | 0.0173 - 0.0202 lb/in³ | ASTM D1895 |
LG Chemical LS100S PVC General Description: LS100S, homopolymer made by suspension polymerization, can be applied to soft or semi-hard products. Products made from LS100S have excellent surface, bright color and transpare.. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | ASTM D1895 |
Plenco 7202 Phenolic, Granular, Injection Molded PLENCO 07202 is an organic fiber reinforced phenolic molding compound, formulated to offer improved mechanical strength properties with an industrial finish. UL recognized under component file E4065.. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | |
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | |
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | |
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 680M PVC Homopolymer General Purpose Grade Resin F680M is a medium molecular weight PVC homopolymer suitable for both rigid and flexible applications and is low in gels and finds acceptance in calendered fil.. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | |
Asahi Glass Fluon® CD090 PTFE Coagulated Dispersion Powder Fluon®PTFE coagulated dispersion powders (fine powders) are used for paste extrusion to make tapes, tubes, rods and wire coatings.Information provided by Asahi Glass Company, Inc. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | DIN EN ISO 60 |
3M Dyneon™ TF 2021Z PTFE Fine Powder Dyneon TF 2021 Z PTFE is an ideal grade for pipe liner applications because of its outstanding green strength. It is the preferred grade for unsintered thread sealing tapes, expanded join sealings, .. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | DIN EN ISO 60 |
3M Dyneon™ TF 2025Z PTFE Fine Powder Dyneon™ TF 2025 Z PTFE is an ideal grade for pipe liner applications in chemical plant construction due to high green strength.Product Features:High molecular weightFine powder grade for low to med.. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | |
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Bulk Density | 0.480 g/cc | 0.0173 lb/in³ | Tapped |
Nyco ULTRAFIBRE® II Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |