Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bulk Density = 0.0202 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.560 g/cc
0.0202 lb/in³
Tapped
Nyco NYGLOS® M3 Wollastonite
This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make..
Bulk Density 0.560 g/cc
0.0202 lb/in³
SGL Carbon Group CF 1135 Carbon Filler
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Bulk Density 0.560 g/cc
0.0202 lb/in³
DIN 53466
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound
TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA..
Bulk Density 0.560 g/cc
0.0202 lb/in³
ASTM D1895
Plenco 7591 Phenolic, Briquette, Injection Molded
PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
Bulk Density 0.560 g/cc
0.0202 lb/in³
ASTM D1895
Westlake 1230P PVC
Westlake PVC 1230P resin is a general purpose, medium molecular weight homopolymer designed primarily for the extrusion of rigid PVC products.Information provided by Westlake Chemical Corporation
Bulk Density 0.560 g/cc
0.0202 lb/in³
ASTM D1895
Westlake 1230S PVC
Westlake PVC 1230S resin is a medium molecular weight homopolymer designed primarily for the extrusion of rigid products.Information provided by Westlake Chemical Corporation
Bulk Density 0.560 g/cc
0.0202 lb/in³
ASTM D1895
Formosa Plastics Formolon® 113 PVC
PVC Copolymer Suspension Resin F-113 has been developed primarily to meet the processing requirements of the vinyl composition tile (VCT) manufacturers. In addition to vinyl floor tile industry, F-1..
Bulk Density 0.560 g/cc
0.0202 lb/in³
ASTM D1895
Formosa Plastics Formolon® 614 PVC
Homopolymer - General Purpose Grade Resin F614 is a medium-low molecular weight PVC homopolymer of particular interest in rigid applications and has established a deserved reputation for low gels an..
Bulk Density 0.560 g/cc
0.0202 lb/in³
ASTM D1895
Formosa Plastics Formolon® 622E PVC
Rigid Extrusion Resin F622E is a medium-low molecular weight PVC designed primarily for rigid extrusion applications. This product has excellent dry flow characteristics, making it desirable for dry..
Bulk Density 0.560 g/cc
0.0202 lb/in³
ASTM D1895
Formosa Plastics Formolon® 622R PVC
Homopolymer General Purpose Grade Resin F622R is a medium-low molecular weight PVC homopolymer of interest in both rigid and flexible applications and has established a deserved reputation for low ..
Bulk Density 0.560 g/cc
0.0202 lb/in³
ASTM D1895
Equate EGDA-6888 HDPE Film Extrusion Resin
EGDA-6888 is a high molecular weight, high density polyethylene copolymer that has been designed specifically for tubular film extrusion. Its broad molecular weight distribution and density have bee..
Bulk Density 0.560 g/cc
0.0202 lb/in³
Asahi Glass Fluon® L170J PTFE Lubricant
Fluon®PTFE lubricants are used as additive to plastics, rubbers, paints, greases and so on. Frictional resistance decreases and non-stick increases on the applied surface.Information provided by As..
Bulk Density 0.560 g/cc
0.0202 lb/in³
Asahi Glass Fluon® L172J PTFE Lubricant
Fluon®PTFE lubricants are used as additive to plastics, rubbers, paints, greases and so on. Frictional resistance decreases and non-stick increases on the applied surface.Information provided by As..