Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade
(discontinued **) ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H4262 High Density Polyethylene, Injection Molding Grade
(discontinued **) ApplicationsAlathon H4262 is a high-flow resin that exhibits very good cold temperature impact performance, optimum processing and thermal stability, with good color and organoleptic properties. Typ.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H4250 High Density Polyethylene, Injection Molding Grade ALATHON H4250 is a high-flow “freezer†grade resin that exhibits enhanced cold temperature impact performance, enhanced processing and thermal stability, with good color and organoleptic p.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H4620 High Density Polyethylene, Injection Molding Grade Alathon H4620 is a medium-flow resin that exhibits good cold temperature impact performance, enhanced processing and thermal stability. Typical applications are thinner-walled parts that require che.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade ALATHON H6017 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, c.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® M5352 High Density Polyethylene, Injection Molding Grade ALATHON M5352 is a high density copolymer with a narrow molecular weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good proces.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® M5372 High Density Polyethylene ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. .. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade ALATHON M6080 is a narrow molecular weight distribution homopolymer that exhibits enhanced flow characteristics and good balance of stiffness and impact resistance. Typical applications include case.. |
|||
Bulk Density | 0.593 - 0.625 g/cc | 0.0214 - 0.0226 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H5112 High Density Polyethylene, Injection Molding Grade ALATHON H5112 is a medium-molecular-weight-distribution resin with balanced impact/ESCR and high flow characteristics. Typical applications include housewares, food containers, pail handles and toys.. |