Polymer Property : Bulk Density = 0.0324 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.898 g/cc
0.0324 lb/in³
Vibrated (US Produced); ASTM D1895
Eastman CB12 PET  (discontinued **)
Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good ov..
Bulk Density 0.897 g/cc
0.0324 lb/in³
L 150
Indorama StarPet Preformance® 1708 PET Resin
Description: Preformanceâ„¢ PET 1708 is a food grade PET copolymer that is suitable for a wide variety of beverage and juice containers as well as many other containers. It is engineered for heat..
Bulk Density 0.897 g/cc
0.0324 lb/in³
L 150
Indorama StarPet Preformance® ES11 PET Resin
Description: Preformanceâ„¢ PET ES11 is a high intrinsic viscosity food grade PET copolymer that is specially designed for the CSD container market. It offers excellent reheat ability that improv..
Bulk Density 0.897 g/cc
0.0324 lb/in³
QSWI 8.2.4.150
Indorama StarPet Preformance® N2R PET Resin
PREFORMANCE® PET N2R is a food grade PET copolymer specially designed for the water container market. It offers excellent clarity and color and a low acetaldehyde content to help minimize impact ..
Bulk Density 0.897 g/cc
0.0324 lb/in³
Dried at 110°C (230°F)
Skamol Group Skamol M-20 Insulating Mortar
SKAMOL insulating mortars have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Dry-mix mortars designed for use with Skamol insulating bricks/blocks and slab grad..
Bulk Density 0.897 g/cc
0.0324 lb/in³
nominal
Wellman AquaClear® Ti844 PET
AquaClearTI® 844 is a TPA-based polyethylene terephthalate resin made especially for use in the packaging applications. It’s a solid state copolymer resin with an intrinsic viscosity of 0.72. Aqua..
Bulk Density 0.897 g/cc
0.0324 lb/in³
Nominal
Wellman PermaClear™ 61803 (0.81 IV) PET
PermaClear® 61803 is a TPA-based polyethylene terephthalate resin made especially for use in packaging applications. It is a solid-stated copolymer resin with an intrinsic viscosity 0.81 IV. PermaC..
Bulk Density 0.897 g/cc
0.0324 lb/in³
Nominal
Wellman PermaClear™ HP806 (0.84 IV) PET
PermaClear® HP806 is a TPA-based polyethylene terephthalate resin made especially for use in packaging applications. It is a solid-stated copolymer resin with an intrinsic viscosity 0.84 IV. PermaC..
Bulk Density 0.897 g/cc
0.0324 lb/in³
nominal
Wellman ThermaClear® Ti818 (0.79 IV) PET
ThermaClearTI® Ti818 is a TPA-based polyethylene terephthalate resin made especially for use in packaging applications. Its titanium catalyst and copolymer formulation provide outstanding clarity a..
Bulk Density 0.897 g/cc
0.0324 lb/in³
DAK-QAR-SOP-0018
DAK Americas Laser+® C 61803 (E67A) PET
Product Description: Laser+® 61803 (E67A) is a unique copolymer particularly suited for use in the custom PET container applications where clarity and neutral color are desired. It is a medium intr..
Bulk Density 0.897 g/cc
0.0324 lb/in³
DAK-QAR-SOP-0018
DAK Americas Laser+® HP806 (B93A) PET
Product Description: Laser+® HP806 (B93A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Ty..
Bulk Density 0.897 g/cc
0.0324 lb/in³
DAK-QAR-SOP-0018
DAK Americas Laser+® HS Ti818 (G51A) PET
Laser+® HS Ti818 (G51A) polyethylene terephthalate (PET) resin is designed for conversion to PET packaging by injection stretch blow-molding using commercial heat-set technology.Laser+® HS Ti818 (..
Bulk Density 0.897 g/cc
0.0324 lb/in³
DAK-QAR-SOP-0018
DAK Americas Laser+® W Ti844 P46A PET
Product Description: Laser+® W Ti844 (P46A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology...