Physical Properties Metric English Comments
Bulk Density 1.45 - 1.55 g/cc
0.0524 - 0.0560 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 125 GM Refractory Insulating Castable
Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast...
Bulk Density 1.45 - 1.55 g/cc
0.0524 - 0.0560 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 125 Refractory Insulating Castable
Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products. Also available in gunning variety, mar..
Bulk Density 1.45 - 1.55 g/cc
0.0524 - 0.0560 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 140 Refractory Insulating Castable
Description: This castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere.Remarks:..
Bulk Density 1.45 - 1.55 g/cc
0.0524 - 0.0560 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 155 Refractory Insulating Castable
Description: Due to it's high strength at high temperatures, this material can be applied in direct contact with the firing process.Remarks: These values apply to cast products. Also available i..
Bulk Density 1.45 - 1.55 g/cc
0.0524 - 0.0560 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 160 Refractory Insulating Castable
Description: This castable can be used up to very high temperatures under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information..
Bulk Density 1.46 - 1.55 g/cc
0.0527 - 0.0560 lb/in³
3M #14 Roofing Granule (Corona)
3M #14 Grade Roofing Granules are ceramic-coated minerals used as surfacing material in asphalt roofing products.Information provided by 3M
Bulk Density 1.45 - 1.55 g/cc
0.0524 - 0.0560 lb/in³
After drying at 110°C
Gouda Vuurvast GOLITE 135 GM Refractory Insulating Castable
Description: This gunning material can be used in direct contact with open fire and has a high strength.Remarks: These values were obtained from cast samples. These values apply to cast products.Inf..