Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.60 g/cc | 0.0579 lb/in³ | packed |
Imerys Minsparâ„¢ 1 Feldspar Minspar 1 is a minus 30 mesh Feldspar product used in the glass container and ceramic tile markets.Information provided by Imerys |
|||
Bulk Density | 1.60 g/cc | 0.0579 lb/in³ | Dried at 110°C (230°F) |
Skamol Group Skamol FL-06 Insulating Mortar SKAMOL insulating mortars have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Dry-mix mortars designed for use with Skamol insulating bricks/blocks and slab grad.. |
|||
Bulk Density | 1.60 g/cc | 0.0579 lb/in³ | Packed |
Excalibar ExCal® 100 Calcium Carbonate CaCO3 Powder ExCal® calcium carbonate is processed from a high-purity stone, to exacting specifications at the Excalibar Minerals plants. It is suitable for use in plastics, adhesives, sealants, and other appli.. |
|||
Bulk Density | 1.60 g/cc | 0.0579 lb/in³ | Packed |
Excalibar ExCal® CW 100 Calcium Carbonate CaCO3 Powder ExCal® CW calcium carbonate products are processed from a high-purity ore, to exacting specifications at the Houston, Texas plant. These grades are processed for use in plastics, rubber, coatings,.. |
|||
Bulk Density | 1.60 - 1.76 g/cc | 0.0579 - 0.0637 lb/in³ | Nominal |
ATI Wah Chang Hafnium Tetrachloride LZ (Low Zirconium) Grade, HfCl4 A white anhydrous powder.Information provided by ATI Wah ChangTypical Analysis: On Hf metal basis |
|||
Bulk Density | 1.60 - 1.76 g/cc | 0.0579 - 0.0637 lb/in³ | |
ATI Wah Chang Hafnium Tetrachloride, HfCl4 A white, free flowing, anhydrous powder.Information provided by ATI Wah ChangTypical Analysis: On Hf metal basis |
|||
Bulk Density | 1.60 g/cc | 0.0579 lb/in³ | Tapped; ASTM D 3101-78 |
Potters Industries Spheriglass® 3000E Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |