Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.60 g/cc | 0.0578 lb/in³ | Tapped |
Nyco NYGLOS® M50 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 1.60 g/cc | 0.0579 lb/in³ | packed |
Imerys Minsparâ„¢ 1 Feldspar Minspar 1 is a minus 30 mesh Feldspar product used in the glass container and ceramic tile markets.Information provided by Imerys |
|||
Bulk Density | 1.60 - 2.20 g/cc | 0.0578 - 0.0795 lb/in³ | loose |
Solvay Chemicals Barium carbonate granular Barium carbonate granular is used for the production of display glass, crystal glass and other special glass, glazes, frits and enamels. Barium carbonate granular is also used in the chemical indust.. |
|||
Bulk Density | 1.60 - 2.20 g/cc | 0.0578 - 0.0795 lb/in³ | loose |
Solvay Chemicals Strontium carbonate granular Strontium carbonate granular is used in the production of display glass and other glass. Strontium carbonate granular is also used in the metallurgy.Information provided by Solvay |
|||
Bulk Density | 1.60 g/cc | 0.0578 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL 15 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Bulk Density | 1.60 g/cc | 0.0578 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL 15LI Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Bulk Density | <= 1.60 g/cc | <= 0.0578 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFINSUL ZAP-020 Insulating Castables Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l.. |
|||
Bulk Density | 1.60 g/cc | 0.0579 lb/in³ | Dried at 110°C (230°F) |
Skamol Group Skamol FL-06 Insulating Mortar SKAMOL insulating mortars have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Dry-mix mortars designed for use with Skamol insulating bricks/blocks and slab grad.. |
|||
Bulk Density | 1.60 g/cc | 0.0579 lb/in³ | Packed |
Excalibar ExCal® 100 Calcium Carbonate CaCO3 Powder ExCal® calcium carbonate is processed from a high-purity stone, to exacting specifications at the Excalibar Minerals plants. It is suitable for use in plastics, adhesives, sealants, and other appli.. |
|||
Bulk Density | 1.60 g/cc | 0.0579 lb/in³ | Packed |
Excalibar ExCal® CW 100 Calcium Carbonate CaCO3 Powder ExCal® CW calcium carbonate products are processed from a high-purity ore, to exacting specifications at the Houston, Texas plant. These grades are processed for use in plastics, rubber, coatings,.. |
|||
Bulk Density | >= 1.60 g/cc | >= 0.0578 lb/in³ | |
Chosun Refractories IC-RK Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 1.60 g/cc | 0.0578 lb/in³ | |
Chosun Refractories LWB-170 Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 1.60 g/cc | 0.0578 lb/in³ | |
Chosun Refractories MF-2 Blast Furnace Tap-Hole Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 1.60 - 1.76 g/cc | 0.0579 - 0.0637 lb/in³ | Nominal |
ATI Wah Chang Hafnium Tetrachloride LZ (Low Zirconium) Grade, HfCl4 A white anhydrous powder.Information provided by ATI Wah ChangTypical Analysis: On Hf metal basis |
|||
Bulk Density | 1.60 - 1.76 g/cc | 0.0579 - 0.0637 lb/in³ | |
ATI Wah Chang Hafnium Tetrachloride, HfCl4 A white, free flowing, anhydrous powder.Information provided by ATI Wah ChangTypical Analysis: On Hf metal basis |
|||
Bulk Density | 1.60 g/cc | 0.0579 lb/in³ | Tapped; ASTM D 3101-78 |
Potters Industries Spheriglass® 3000E Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |